Good morning gold refining forum! Just wanted to enter some yield data. I recently processed 6.16 lb of goldfingers and other gold-plated items such as SIM cards and other small gold-plated stuff where the gold isn't attached to metal such as pins or jewelry. Ribbon cable ends and things like that. Well I managed to recover 11.6 grams of gold. I had my hopes low so as not to be let down when I got the f yield. But this exceeded my expectations. Can anyone tell me whether or not this is an average yield? They were all closely trimmed.
 
Or about a 0.004 recovered from the fingers or 0.0004 from whole sticks, either way about $100
 