It never occured to me that a stainless steel sink with a plastic 2 way ball valve at the bottom could be used as/for a silver cell. The electrolite could be filtered and removed at the bottom by one direction of the valve, leaving the silver to be washed directly in the sink, and the washwater redirected to wastebucket by the 2nd direction of the valve. Hmm.

Thanks for the ideea. :)
 