Palladium Well-known member Joined Jan 17, 2008 Messages 5,724 Location USA Oct 26, 2009 #21 If he boiled all that slag in con sulfuric wouldn't it remove most of the borax ? Then clean it up with some hcl to remove the base metals and then use the acid Clorox process ? Just guessing here. :?:
If he boiled all that slag in con sulfuric wouldn't it remove most of the borax ? Then clean it up with some hcl to remove the base metals and then use the acid Clorox process ? Just guessing here. :?:
Q qst42know Well-known member Joined Jul 16, 2008 Messages 2,963 Location Toledo, Ohio, USA Oct 26, 2009 #22 Unless you added a huge amount of borax, the melt may be mostly Shor gold dissolving salt and precipitant. Is the slag soluble in boiling water?
Unless you added a huge amount of borax, the melt may be mostly Shor gold dissolving salt and precipitant. Is the slag soluble in boiling water?