A Anonymous Guest Nov 15, 2007 #1 I am very intrested in refining cpu's. I have about 50 pounds and cant wait to get started. Any help would be great!
I am very intrested in refining cpu's. I have about 50 pounds and cant wait to get started. Any help would be great!
Noxx Well-known member Joined Feb 24, 2007 Messages 3,365 Location Quebec, Canada Nov 15, 2007 #2 There is plenty of information already posted on the subject. Just do a Search. I recommend using Aqua Regia.