i have just started using house hold bleach and it is eating all the gold from the cpu pins and motherbourd pins and plateing it has gone really black and you can see all the gold specs of plating floating around does some one know how i percipatate the gold from bleach what do i add next any help would be muchly apreciated thanks matthew ps i dont know how to use this web site im very new to this site
 

Claudie

Well-known member
Joined
Aug 17, 2010
Messages
1,853
Location
Iowa
Are you planning on getting a patent on that process? I think you posted in the wrong part of the forum, maybe someone can move it. I think you should put the solution in a safe place and read some of the posts here to learn the right way of getting your Gold back.
Try starting with this link http://goldrefiningforum.com/phpBB3/viewtopic.php?p=6873#6873
 