Hey guys,

Ok I have these old intel chip which I though they where ceramic but they are fiber but weird let me show u


So if u look that is what I have they look like they have gold bonding wire is this true
 

Attachments

  • image.jpg
    image.jpg
    2.2 MB · Views: 31
  • image.jpg
    image.jpg
    1.9 MB · Views: 28

galenrog

Well-known member
Joined
Jan 16, 2010
Messages
658
Location
Oregon
Generally referred to here as black fiber CPUs. Over the years, a few dozen threads have cropped up regarding them. The search function should be helpful to locating some of those threads. Since I do not process electronic scrap, I will be of no help otherwise.

Time for more coffee.
 

galenrog

Well-known member
Joined
Jan 16, 2010
Messages
658
Location
Oregon
When I accumulate a few kilos, I either offer them here, or sell to a company such as Boardsort. Have fun.

Time for more coffee.
 

speed

Active member
Joined
Aug 13, 2017
Messages
30
Yes they have gold bond wires. The central section is basically the same as a normal IC chip and can be processed in the same way. The rest is tricky to process economically.
 

timsiggins

Active member
Joined
Oct 4, 2021
Messages
44
I was able to pull the center out a look at it with a micros scope they have gold bond wires but so short
 