jbollinger97
New member
Hi All,
First post here and hoping you'll be able to provide some input. Been trying to identify if some alloy bars may actually contain Ir and if I should trust the readings. 10 bars have been tested by both a handheld XRF analyzer as well as drill samples were taken and then analyzed with an SII SEA5120A lab xrf spec. Both came up with similar results for this concentrated ore.
18-20% Ir
3-4% Au
55-63% Cu
14-16% Pb
Thanks in advance,
JB
First post here and hoping you'll be able to provide some input. Been trying to identify if some alloy bars may actually contain Ir and if I should trust the readings. 10 bars have been tested by both a handheld XRF analyzer as well as drill samples were taken and then analyzed with an SII SEA5120A lab xrf spec. Both came up with similar results for this concentrated ore.
18-20% Ir
3-4% Au
55-63% Cu
14-16% Pb
Thanks in advance,
JB