- Joined
- Jun 14, 2021
- Messages
- 76
Ok after three years of studying, reading Hokes book and watching god knows how many youtube videos I have finally started, all has went well apart from set up cell at 3.5 constant volts and the amps were sitting at 7.4 amps last night, went to bed and when I got up my full anode basket was empty and my anode bar was eaten away to almost nothing, I have turned the volts down to 1.5v and the amps are sitting at 4.3, hopefully this will slow the rate at which my silver shot is being eaten, Im quickly running out.