I first was on the impression that this was plastic, as this was the body of the pen from an old digitizer.
When i then pick the parts apart i accidently droped it on a wooden floor, and the sound it gave when it hit the floor took me by surprise.
It sounded like an instrument, almost like a tuningfork.
It was coated with a really thick layer paint, and under is a shiny white metal.
I tried heating it and it became maleable when heated with a butan torch , the paint took the fire like a champ , ( yes i use ppe ).
Not magnetic, Have not tried paramagnetism yet, i think i will.
I have a clue what tis could be, but i am real curiuos what you experts think.

Best regards to all of you / Arne
 

Attachments

  • IMG_20240904_221747.jpg
    IMG_20240904_221747.jpg
    2.3 MB
  • IMG_20240904_221747.jpg
    IMG_20240904_221747.jpg
    2.3 MB
  • IMG_20240904_221757.jpg
    IMG_20240904_221757.jpg
    2.3 MB
  • IMG_20240904_221815.jpg
    IMG_20240904_221815.jpg
    874.8 KB
I first was on the impression that this was plastic, as this was the body of the pen from an old digitizer.
When i then pick the parts apart i accidently droped it on a wooden floor, and the sound it gave when it hit the floor took me by surprise.
It sounded like an instrument, almost like a tuningfork.
It was coated with a really thick layer paint, and under is a shiny white metal.
I tried heating it and it became maleable when heated with a butan torch , the paint took the fire like a champ , ( yes i use ppe ).
Not magnetic, Have not tried paramagnetism yet, i think i will.
I have a clue what tis could be, but i am real curiuos what you experts think.

Best regards to all of you / Arne
In the pictures it look like Copper.
 
Last edited:
need weight.
similar to nickel silver, an alloy of nickel, zinc and copper... with a high nickel content.
maybe that’s why it’s painted over, many people are allergic to nickel
 
Hmmmm,,Silver colored metal. My guess would be one of the elements, or an alloy, from the periodic table. No guessing, have it analyzed with an XRF, or run the gamut of acid tests, streak test, hardness, and melting point tests. Just like what you would do to determine a mineral.
 
Its light, Lighter than aluminium.
Scratches easy but quite rigid.
Not copper yggdrasil
I've sometimes found aluminum-magnesium alloys in older equipment. Sometimes even painted parts seemingly made of pure magnesium, which burns white hot when hit with a torch... and I expect must have caused some issues in the buildings where such equipment was used if ever there was a fire!
 
where does beryllium come from?
the world has gone crazy...
Some see a nugget of rhodium in every stone, others find rare beryllium everywhere, the toxicity of which has been known for a hundred years...
an ordinary aluminum-magnesium alloy, like the one beer cans are made from...
 
I've sometimes found aluminum-magnesium alloys in older equipment. Sometimes even painted parts seemingly made of pure magnesium, which burns white hot when hit with a torch... and I expect must have caused some issues in the buildings where such equipment was used if ever there was a fire!
If it is lighter than (a comparable sized) Aluminium tube, it can not be a Precious Metal. There are not low-density PMs.
 