Good Morning all,

I am introducing oxygen into my Crucible during the melting process and I was wondering what would be the best option for the tubing/pipe that is carrying the oxygen. The temperatures in the crucible are getting anywhere from 900 to 1500 C. Would stainless be the best option for this?

Thanks

Glen
 
butcher said:
i would use a ceramic clay pipe


etack said:
Use a quartz tube it has a 1600c melting point and is less effected by fluxes than ceramics.

Eric

Thanks for the suggestions! I really appreciate it. I take a look at some options for those and come up with a plan.

Thanks again!

Glen
 