alexanderclausen651@gmail
New member
Hello everybody Merry Christmas. I am new at Gold reclining and I've been attempting gold extraction from a variety of different electronic components fingers, chips etc. I unfortunately I added everything all together in an AP solution and have been unable to recover the gold flakes because they seem to be suspended and some sort of fibrous copper and who knows what other metal substance I'm unable to filter without collecting everything in that fibrous mess. I'm attempting now to heat the solution in hopes of it dissolving everything. My question is do I have a chance at recovering the gold or is it a loss. Your help is much appreciated thank you