Hi guys. So I did something rather bone headed apparently and am in desperate need of some guidance. So I started this hobby about a year ago wasted alot of material as I was learning, and when I started producing good results, I decided to take all of the gold I processed after each drop, and basically save it in a wine jug roll I saved enough to make a really nice little bar. So I saved and saved, and finally a few days ago, I decided I was going to melt it down. I decanted the water it was in and redissolved it all together, and basically refined it one final time as a whole, washed it a few times, all that good stuff, and dried it and placed it In a crucible. My first bone headed mistake was not weighing it. But it was a really decent amount. What I can say, is I bought the 3 pack of crucibles from Amazon that have 3 sizes for gold and silver melting. It completely filled the smallest one up and I had more left over, so I put it all in the medium size, and it was still too much. I split it in half and started melting it with my map gas torch. I DID glaze the crucible first. So I put a couple of pinches of borax on it after it started turning red, and it started melting about 15 minutes later. As it melted, the size reduced drastically, so I threw the rest of the gold on top of it. Not wanting it to blow away, I added more borax. I might have gone a bit overboard though, because the amount I poured ended up completely covering the gold. So I'm watching the gold melt and start to flow into the borax and my dang torch dies. I decided to fire up my heat treating furnace that I use for knife making, which I HAVE uses as a foundry before to melt silver, and it worked well. So I put the crucible ful of my gold covered with borax. I heated it till the contents were liquified, and kept it in there a bit longer. When I pulled it out I pattempts to pour me contents into a mold, but w) asn'tl quick enough. So it has dried in the crucible leaving me with what seems like a chunk of glass with my gold trapped inside. It's also stuck to the crucible. I can't get it out. Any ideas?