I just try my first x ray today and I watch this video "Silver Recovery From X ray Film COMPLETE PROCESS" how to do it. The first x ray sheet been in the bleach for 15min and it hasn't remove anything yet. I have about 1.5 pound and it it works I will get more to do.
I have a 2 gallon bucket with 1 gallon of bleach. Since it pure Silver I want to make a Sliver Bar and Electrolyte for the Silver Cell. The bucket is outside I will check it when I get up to see if it did work or not.
Any idea that I can do?
EDIT:
Would 100% Nitric Acid work better?
I have a 2 gallon bucket with 1 gallon of bleach. Since it pure Silver I want to make a Sliver Bar and Electrolyte for the Silver Cell. The bucket is outside I will check it when I get up to see if it did work or not.
Any idea that I can do?
EDIT:
Would 100% Nitric Acid work better?