• If you have bought, sold or gained information from our Classifieds, please donate to Gold Refining Forum and give back.

    You can become a Supporting Member or just click here to donate.

For Sale Selling Everything for Metal Processing

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Joined
Apr 1, 2022
Messages
38
Location
Miami
I finally finished my task of converting sterling silver into pure silver bars.
Now i'm selling ALL my equipment CHEAP ! ALL You need ,One big package !
Includes: Electric Furnace 3kg up to 1150 C
Plenty of Crucibles, 3 crucible thongs
Variety of Graphite Molds
Electric Voltage regulated Power Supply
Protective gear, googles, mask, Apron, Gloves , more masks and gloves (than in the pictures)
Glass stir rods, at least 4to 5
All the Lab Glass ware, Buchner tunnels, Flasks, Filter Paper, two packs unopened
Hemostatic pump to empty acids from containers without spilling
Vacuum Pump for Buchner funnel gravity filter
Electric Magnetic Stirrer
Propane Gas Bottles at least 4, some full some half full or more
Gas Torch Pistol
Borax Flux powder
Precision Scale
I'll add also a stainless steel bowl with cover (to build the perfect silver cell)
And other accessories i might find when packing.

Everything is used ( a tad dirty now ( but all in working condition.
Everything you need to produce beautiful ingots like the one in the pic.

i also attached a few pics of the process.. WhatsApp Image 2023-01-29 at 8.53.05 AM.jpegWhatsApp Image 2023-01-29 at 8.53.06 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.06 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.06 AM (3).jpegWhatsApp Image 2023-01-29 at 8.53.06 AM.jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (3).jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (4).jpegWhatsApp Image 2023-01-29 at 8.53.07 AM.jpegWhatsApp Image 2023-01-29 at 8.53.08 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.08 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.08 AM.jpegWhatsApp Image 2023-01-29 at 8.53.09 AM.jpegWhatsApp Image 2023-01-29 at 8.53.12 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.12 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.12 AM (3).jpegWhatsApp Image 2023-01-29 at 8.53.12 AM.jpegWhatsApp Image 2023-01-29 at 8.53.15 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.15 AM.jpegWhatsApp Image 2023-01-29 at 8.53.17 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.17 AM.jpegWhatsApp Image 2023-01-29 at 8.53.18 AM.jpegWhatsApp Image 2023-01-29 at 8.53.19 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.19 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.19 AM.jpeg20230114_152912.jpg20230114_152924.jpg

Taking Offers , payment via Zelle please.
WhatsApp Image 2023-01-29 at 8.53.05 AM.jpegWhatsApp Image 2023-01-29 at 8.53.06 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.06 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.06 AM (3).jpegWhatsApp Image 2023-01-29 at 8.53.06 AM.jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (3).jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (4).jpegWhatsApp Image 2023-01-29 at 8.53.07 AM.jpegWhatsApp Image 2023-01-29 at 8.53.08 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.08 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.08 AM.jpegWhatsApp Image 2023-01-29 at 8.53.09 AM.jpegWhatsApp Image 2023-01-29 at 8.53.12 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.12 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.12 AM (3).jpegWhatsApp Image 2023-01-29 at 8.53.12 AM.jpegWhatsApp Image 2023-01-29 at 8.53.15 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.15 AM.jpegWhatsApp Image 2023-01-29 at 8.53.17 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.17 AM.jpegWhatsApp Image 2023-01-29 at 8.53.18 AM.jpegWhatsApp Image 2023-01-29 at 8.53.19 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.19 AM (2).jpegWhatsApp Image 2023-01-29 at 8.53.19 AM.jpegWhatsApp Image 2023-01-29 at 8.53.18 AM.jpegWhatsApp Image 2023-01-29 at 8.53.17 AM.jpegWhatsApp Image 2023-01-29 at 8.53.17 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.15 AM.jpegWhatsApp Image 2023-01-29 at 8.53.09 AM.jpegWhatsApp Image 2023-01-29 at 8.53.08 AM.jpegWhatsApp Image 2023-01-29 at 8.53.07 AM.jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (4).jpegWhatsApp Image 2023-01-29 at 8.53.07 AM (3).jpegWhatsApp Image 2023-01-29 at 8.53.19 AM (1).jpegWhatsApp Image 2023-01-29 at 8.53.19 AM.jpeg
 
Back