I recently de-plated some silver there wasn't much but I depleted it and I washed it and then washed it with hydrochloric acid and then wash it again with boiling water multiple times. But when I went to go put in the sodium hydroxide everything turned reddish or dark red. Is anybody have any idea where I went wrong and what I could do to fix it?