The box was about the size of a shoebox that a pair of boots would come in, square not rectangular. Pretty simple. The furnace was a big gas fired muffle furnace which had doors on both ends. The giant cupel was slid into the furnace and charged from a port in the top. I don't have any pictures but the design was identical to the style often shown in old assay books.