I'm certainly not one to be giving advice but, more information is needed.
Check out the info Lazersteve has, on rhodium testing.
What kind of solution is it and what was it produced from?
I've never experienced a stannous test like you've described.
Did you test your stannous on a known pm solution?
Mark