Jram3105

Member
Joined
Jan 3, 2022
Messages
8
Location
York, SC
I had something happen today that I've never had happen before.... I placed my scrap inside my purified water and as soon as I added my nitric acid to it, the liquid became a dark red and was very thick. I also noticed that the bubbles were having a hard time popping and going down because it was so thick. Has anyone else had this issue before and if so what caused it? Thanks so much for the help.
 