Z zamistro Well-known member Joined Sep 29, 2009 Messages 52 Oct 30, 2009 #1 I'm about to try my hand at some CPUs and fingers. I'm leaning toward the Poor Man's Aqua Regia method, but is there a more fool proof way to do this?
I'm about to try my hand at some CPUs and fingers. I'm leaning toward the Poor Man's Aqua Regia method, but is there a more fool proof way to do this?
A Anonymous Guest Oct 30, 2009 #2 hcl and peroxide for the fingers, I guess the poor mans for the cpu would be normal, keep as much solder and lead out of the reactions. Jim