For those who have not already seen it, this is a three part series I made for my youtube channel about the Wohlwill process. I got a fantastic result. I may have to repeat this in a future all-in-one video. Thanks for looking.

Wohlwill process part 1, Making the electrolyte: https://youtu.be/6gSShkk4-dI

Wohlwill process part 2, Operating the cell: https://youtu.be/zDfujDqEPMo

Wohlwill process part 3, Melting the gold: https://youtu.be/BkvYip3PlhA
 