-rob-
Member
Very true!
Good information. Thank youwell im willing to tell u where i get mine and without being a jerk about it.
i usually look in garage sales and swap meets . and there are still some bargains to be found on ebay , theyre just very far and few between.
today a package came from ebay . 750 grams of memory boards , which cost me $21 plus $9 postage . so for $30 i got a nice pile of fingers and ic chips . plus theyre old ram sticks which have gold all over them , not just fingers.
and at $53 per gram in australia . ill double my money almost if i can get just 1 gram.
it is a fun hobby . ive been at it for years . and like the others have said , good deals dont jump out at ya . you need to have one eye open all the time .i wish you luck finding the good deals , they are out there . u just have to find them.
good luck and i hope it works out for you.
my advice is , while youre looking for material , study the process because its not as easy as it looks . and take it from me , people on here have attitude when you ask for help . i know cuz its all i get.
i think youre better off stock piling it when you do find it . and really getting to know exactly what youre doing , so that when you do start , it will be joy instead of a nightmare.
So, I've used the HiBid auctions site. I've acquired a little bit, set a price I'm comfortable with and don't chase. Unfortunately for me, I'm still full time work (60 hours a week), though getting ready to slow down /semi retire. Just in the collection mode, so all the discussions are good.Finding materials to recover and refine has always been one of the hardest parts of this as a hobby or even a business many members are lucky to refine an ounce of gold a year.
There is material out there but finding the sources can be utterly frustrating to be polite but as I have said before talk to everyone you know or meet about your new hobby and what you are looking for, you really never know where that connection will be made .
Not Amazon or EBay. Do a Google search for chemistry lab glassware. I can’t remember the names, but there are a few with anything you might need or want.So, I've used the HiBid auctions site. I've acquired a little bit, set a price I'm comfortable with and don't chase. Unfortunately for me, I'm still full time work (60 hours a week), though getting ready to slow down /semi retire. Just in the collection mode, so all the discussions are good.
I did see a few auctions of larger lots of silver, decently priced to start with. Then it gets run up, so now looking at other places in around Lost Wages.
Now the question I have is lab materials. Is there a decent place to purchase from (all the glass & chemicals, fume hoods)? I've seen a big disparity on ebay/Google.
Thank you
I've been saving electronic scrap for years, cleaning it up as I can. Only now am I finally starting to move towards refining the precious metals out.
I'm starting with silver and copper, because if I screw up royally the losses will be under $1 a gram. And there's how incredibly competitive everyone is for gold these days! If you can't afford to pay the price gold is selling at, you certainly can't afford to risk losing it because you made a mistake with the chemistry.
Start with silver. Learn to handle the chemicals safely and determine if this work is something you're sincerely invested to do. Gather gold as you can while you're learning. It's value isn't going to drop. Once you can safely process silver and get your expected yields, you'll probably be ready to move to gold.
Yes sir, it's a Falcon metal detector pin point probe. I got it in Arizona about 8 yrs ago.@campbellj46,
Could you explain what the little electronic black box with the two knobs is in your 022218.jpg? I'm assuming it's some sort of metal detector? Could you let us know what it is? Thanks.
@campbellj46,
I found a few videos on it to share with the forum. Thanks for posting what is it, I'm always excited to see some of the tech people use to help them in the precious metal work.
Falcon MD20, how to find gold on bedrock with a metal detector.
Gold Prospecting Falcon MD 20 Metal Detector
Tuning the Falcon MD20 - Fixing if it squeals all the time
Falcon Metal Detector--Gold mining tutorial
Welcome to us.I am Sundar Tumuluru from Chennai, India and would like to join the bandwagon of Gold refining forum as I am also have 2 doctorates in Chemistry and Business Mgmt.
My wife passed away 8 months back and my children are well settled, now wanted to make a Hobby out of GOLD REFINING.. What are the Suggestions to start with....expect themembers to assist me in this hobby, though it is a costly one, have no liabilities to continue.
I am in the exact same boat here. Trying to find another hobby during these crazy times and I'm not even looking to make any money off of it. I'll be happy if I just break even, i just wanna do it for fun. Cuz who doesn't want to pour their own ~24k gold?! I've bid on numerous auctions on Ebay and have yet to win a single one of them. Every one I see, the scrap goes for either exactly scrap price or even over. I'm trying to get scrap for at most 90% of its value, because when I turn around to sell it I'm sure I won't even get that much back. But like I said it'll be a fun hobby when I can get my hands on some scrap and hopefully it'll be a hobby that will be close to paying for itself!
Enter your email address to join: