Topekole Member Joined Nov 24, 2018 Messages 11 Dec 12, 2018 #1 I got this from an old printer look lie it is good plated, please help me to check it is worth keeping? Thanks Attachments IMG_20181212_111043_521.jpg 130.8 KB · Views: 184 IMG_20181212_111012_035.jpg 642.1 KB · Views: 184
I got this from an old printer look lie it is good plated, please help me to check it is worth keeping? Thanks
K kurtak Well-known member Joined Jan 16, 2014 Messages 3,846 Location John Day Oregon Dec 12, 2018 #3 Dr.xyz said: No. Click to expand... No is the right answer - it's brass Kurt