Hello I have hung o to these boards for some time now and would like to clear up some space.There is about 100 ofor each board .any help would be greatly appreciated.

Matt

AI-712 -100 20200416_225232196.jpg
Power control boards -80 View attachment 2
IEE / Canstar 80 - 20200416_225303412.jpg
 

Attachments

  • 20200416_225246711.jpg
    20200416_225246711.jpg
    419.8 KB · Views: 196
Bottom is power grade.
Next one up is power grade or mid grade, depending on connectors on the end.
Top board is hard, it's either going to go low tel or mid grade, depending on weight of the board. I'd personally call it low tel, but I'm not a buyer. It all depends on the thickness of the board itself.
 