Photos of Types of Scrap

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

goldsilverpro

In Remembrance
Moderator Emeritus
Joined
Mar 30, 2007
Messages
7,961
Location
Benton, Arkansas
Great photos. If you've never seen photo silver flake, Pt thermocouple wire, Pt labware, Pt catheters, and bench sweeps and filings, here's where to see them. I can't believe I haven't seen this page before.

http://www.midwestrefineries.com/imagegallery.htm
 
Do you think this medical grade wire I have pictured below could be the kind they talk about?
Just have to see if anyone knows before scrapping out as insulated wire. :)
Thanks
 

Attachments

  • 108_1374.jpg
    108_1374.jpg
    312.2 KB · Views: 1,402
Charlena,
When in doubt about any wire try it in nitric acid,
or your acid from gold test kit. If it survives the
acid test it isn't copper. Medical stuff I would say
you never know, but mainly high temperature
applications will have the platinum thermocouple
wire. Jim
 