Sodium Bisulfate (NaHSO4)I thought for sure i would see something about this on here,but nothing.Kind of researching in general.Any insights?
 
butcher said:
NaHSO4 makes a very good substitute for sulfuric acid in reactions.
At my local lapidary guild, we use sodium bisulfate for our silver pickle, and I take it home and dispose of it in my refining waste stream. But now I'm wondering if I can use it for silver chloride conversion with iron. Does that sound reasonable?
 
Topher_osAUrus said:
Yet another way for converting AgCl.
Brilliant!
Aye, and reusing a waste solution to boot!

It's dirty pickle, but the silver chloride I'm looking to convert is actually from my stock pot, so I was going to redigest it in nitric regardless.
 