kjavanb123
Well-known member
All
Perivously on my telecomm boards post, I generated 1.5 gallons of cyanide waste solution, which I tried to decompose based on my understanding of GoldSilverPro's post. Please comment.
Here is the waste cyanide solution,
Inserted 2 stainless steel rods from computer scraps,
Power it up at 6V, 4A, white foams apperraed from rod to another and I left there.
Thanks
Kevin
Perivously on my telecomm boards post, I generated 1.5 gallons of cyanide waste solution, which I tried to decompose based on my understanding of GoldSilverPro's post. Please comment.
Here is the waste cyanide solution,
Inserted 2 stainless steel rods from computer scraps,
Power it up at 6V, 4A, white foams apperraed from rod to another and I left there.
Thanks
Kevin