Hello friends.
I want to share how to burn activated carbon with gold.
There is much talk of burning gold activated carbon. That is very difficult but if first ground and form a pellet in the following proportion can be performed easily.
The coal is agglomerated with a mixture of
5 liters of water
600g of sodium nitrate
200g maltodextrin
The pellet dry and burn easily
Good luck
I want to share how to burn activated carbon with gold.
There is much talk of burning gold activated carbon. That is very difficult but if first ground and form a pellet in the following proportion can be performed easily.
The coal is agglomerated with a mixture of
5 liters of water
600g of sodium nitrate
200g maltodextrin
The pellet dry and burn easily