Has anyone ever cd's or cd-r's or similar recycled?
I found nothing with the Forum search.
I found an article at the web about this sorry it's in german but maybe google translation service helps a little bit.
http://www.ruhr-uni-bochum.de/rubin/rbin2_01/studieren/index.html
I find this interesting because old cd's are available everywhere.
Best Regards
Tommy
edit: According to report are 10 mg of silver or 9 mg of gold per cd included depending on the type.