goldfever007
Active member
- Joined
- Mar 22, 2018
- Messages
- 39
Dear member:
First of all let me thank you all for sharing the knowledge.....
Second i was always wondering ,when we add copperas or SMB to AR ,why we have to wait till tomorrow or hours ? why don't we use heat so we can recover the gold quickly?
First of all let me thank you all for sharing the knowledge.....