Mountain Man
Well-known member
- Joined
- Sep 11, 2016
- Messages
- 102
I have a question. I have a friend who says he has a mix of material that he wants me to process for him.
He claims he has had the material assayed and it came back as 50% pure gold and 50% platinum. My question is how do I separate the gold from the platinum and how do I process the platinum once they are separated? I know nothing about processing platinum or the best way to separate the 2. He claims he has a pound of the material.
I would be very grateful for any and all advice on the method of separation and recovery of the 2 materials.
Thank you for your help.
He claims he has had the material assayed and it came back as 50% pure gold and 50% platinum. My question is how do I separate the gold from the platinum and how do I process the platinum once they are separated? I know nothing about processing platinum or the best way to separate the 2. He claims he has a pound of the material.
I would be very grateful for any and all advice on the method of separation and recovery of the 2 materials.
Thank you for your help.