A while back I ran some gold over silver material and used nitric acid to dissolve the silver from the gold. It has been sitting and some of it has evaporated down and it started to drop out some whitish/silver looking crystals. I would like to use the left over solution in a cell to break down some more sterling if possible and if not I still need to recover the silver. How would I redissolve the crystals to make it usable, or is it even necessary to put those crystals back in solution? The original solution was just over 4 oz of sterling in 850 ml of 68% ntiric and distilled water at a ratio of 1:1. It is now down to just over 500ml.
Sorry, I am not very up on silver and need to start learning more about it.
Sorry, I am not very up on silver and need to start learning more about it.