Here's a video I did to show how I double refine some 14k and 10k gold scrap jewelry:
Some borax came over with the pour and glued the gold bar in the graphite mold
Had to break it to get the gold out!

https://youtu.be/9NzAdQZcJv0

kadriver
 
Damn you make some good videos. I actually watched the whole thing, what a marathon, I'm surprised you stayed up to do it.
 
I do try to keep the video area clean. It looks better if I do a little prep work before I begin shooting video.