I've seen a setup somewhere where this guy had a 4L erlenmeyer flask along with a glass stopper on top that has two holes for the condenser and the doser.

What do you call the glass stopper with two holes and the doser?

The doser is like a small pvc ball valve with a funnel on top. You could add small doses of chemical in the funnel and then open the ball valve.
 
By "doser", do you mean a "pressure equalising dropping funnel"? A "separatory funnel" designed for another purpose may often also be used as a dropping funnel, but lacks pressure equalisation.
 
even a claisen adapter with a equal pressure addition funnel and a reflux condenser would accomplish his goals...
 
Claisen adapter! Yes! Thank Lou!

Now to perfect the system how do I go about mixing?
I usually open the stoppers and put a polypropylene pipe to mix. What do you guys do?
I do not think a magnetic mixer will survive the nitric / ar digestions or would it?
 
autumnwillow said:
Claisen adapter! Yes! Thank Lou!

Now to perfect the system how do I go about mixing?
I usually open the stoppers and put a polypropylene pipe to mix. What do you guys do?
I do not think a magnetic mixer will survive the nitric / ar digestions or would it?

There are coated mixers that will stand up to the AR and other chemicals. You can find them in ebay and other places.
 
PTFE / PPR coated mixers.

Won't that get damaged from inquarted cornflakes immediately?
Or can it survive at least a few mixes before it wears out?
 
If it's inquarts and you're doing nitric, just use stainless 304L.

If it's inquarts then aqua regia in same reactor, use CP titanium.


Lou
 
For a small bid I won 9 of these 3L and6L Wheaton Magnaflex bottles and have been searching for their purpose and possible use in refining.
http://goldrefiningforum.com/phpBB3/download/file.php?mode=view&id=33493
 

Attachments

  • 1323217.jpg
    1323217.jpg
    30.5 KB · Views: 125
Lou said:
If it's inquarts and you're doing nitric, just use stainless 304L.

If it's inquarts then aqua regia in same reactor, use CP titanium.


Lou

What I meant was the magnetic stirrer bars not the container.
 