Hi everyone
Im new to this forum but i have been looking around and i must say there are a lot of interesting posts and good information here.
I have been thinking about starting a real business scraping electronics. More specificaly PCBs. I searched the forums for information about electrostatic separation and did not find much.
So far i have been in contact with one company that specializes in this kind of separation, http://www.ife-system.se. They told me that the best solution if using this method is to grind the material to a very fine grade. Less than one mm in size (less than 0.04 inches).
Then the separation process will be the most accurate.
It will separate into no-metalic and metalic particles. And refinment will take on from there.
Do anyone have experience with this sort of machines and could provide some input or thoughts?
Thanks alot!
Im new to this forum but i have been looking around and i must say there are a lot of interesting posts and good information here.
I have been thinking about starting a real business scraping electronics. More specificaly PCBs. I searched the forums for information about electrostatic separation and did not find much.
So far i have been in contact with one company that specializes in this kind of separation, http://www.ife-system.se. They told me that the best solution if using this method is to grind the material to a very fine grade. Less than one mm in size (less than 0.04 inches).
Then the separation process will be the most accurate.
It will separate into no-metalic and metalic particles. And refinment will take on from there.
Do anyone have experience with this sort of machines and could provide some input or thoughts?
Thanks alot!