Good day!
I have about 120 grams of extremely fine silver and gold shavings from a jewelers bench, of which silver is the higher concentration (60/40).
Can someone assist me in a method of extracting the gold from the silver w/o the use of nitric acid? Nitric acid is not readily available in my neck of the woods.