More eye candy!

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Thank you all!
It's gold recovered from military/aerospace pins...
I like to melt them and run them thru P.AR ... the acids attack the base metals more readily. I run them thru AR for final refining.
That's the second batch; and more still to come in the next few months!

Thank you, GRF!

Phil
 

Attachments

  • IMG_2818.JPG
    IMG_2818.JPG
    659.6 KB · Views: 347
philddreamer said:
Thank you all!
It's gold recovered from military/aerospace pins...
I like to melt them and run them thru P.AR ... the acids attack the base metals more readily. I run them thru AR for final refining.
That's the second batch; and more still to come in the next few months!

Thank you, GRF!

Phil
wow nice buttons..... wish I knew what to do with my growing collection of bits and crumbs ... for now looking at them makes me think I've what You have " PhDRMR " but I know theres work to do first... .. ( Suggestions are very Welcome )
 

Attachments

  • IMG_1599.JPG
    IMG_1599.JPG
    684.7 KB · Views: 246
  • IMG_1603.JPG
    IMG_1603.JPG
    588.5 KB · Views: 246
  • IMG_1604.JPG
    IMG_1604.JPG
    566.9 KB · Views: 246
  • IMG_1605.JPG
    IMG_1605.JPG
    578 KB · Views: 246
  • IMG_1611.JPG
    IMG_1611.JPG
    754.3 KB · Views: 246
Most of what you have looks like good candidates for the sulfuric stripping cell, most of what you have is nowhere near as good as Phil’s material unfortunately but keep at it you may well find a sweet deal yet.
 