Cemented Silver

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Geo

Well-known member
Joined
Mar 1, 2011
Messages
7,070
Location
Decatur,Ala.
Cemented silver from various sources. Assayed at 99.6% silver.
 

Attachments

  • 100_1883.JPG
    100_1883.JPG
    267.5 KB · Views: 265
  • 100_1884.JPG
    100_1884.JPG
    278.5 KB · Views: 265
I'm calling you out, Geo. That little bar on the right is too yellow. There's no way that's 99.6% silver.

It's still a nice part of the collection though :D
 
Yea, the little one was a little contaminated. 99.1% gold and .9% silver. It was really bad. :-D
 