Postby Goldextraction32 » September 16th, 2018, 12:55 pm

We have a gold cyanide solution of 28 liters. We removed gold from gold plated connectors. We used 475 grams of commercial grade sodium cyanide and 5 liters of hydrogen peroxide of 36%. This solution contains 100 grams of gold & around 5 grams of iron. Can sodium cyanide and hydrogen peroxide be destructed using copper sulfate & sodium metabisulfite ? Or there could be a better solution ? How much quantity of chemical/chemicals will be used to destroy sodium cyanide and hydrogen peroxide? How to proceed about it?
Please Help !


User avatar
FrugalRefiner
Active Member
Posts: 3603
Joined: January 14th, 2012, 5:06 pm
Country of Origin: USA
Location: Ohio, USA

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby FrugalRefiner » September 16th, 2018, 2:09 pm

Goldextraction, you should never start any process without a complete understanding of all the safety aspects, including how to deal safely with the waste, especially cyanide!

I can't answer your question as I don't personally use cyanide, but I'm sure someone will be along soon who can.

Be safe.

Dave
Printer friendly copy of C. M. Hoke's Refining Precious Metal Wastes.
Screen readable copy of C. M. Hoke's Refining Precious Metal Wastes.

User avatar
Platinum
Active Member
Posts: 57
Joined: January 3rd, 2008, 4:26 pm
Location: Earth

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Platinum » September 16th, 2018, 3:31 pm

I'm also a member over at 911 Metallurgist. Is this the same discussion from over there about the gold fingers?
The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C[1].M Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/lndylk
4. Chemistry Handbooks Here (FREE) >> http://tinyurl.com/n27pqu
ALL FREE-----ALL THE TIME

Lino1406
Active Member
Posts: 1249
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Lino1406 » September 16th, 2018, 10:42 pm

Hypochlorite will destroy cyanide. (Air) mixing and enough time - meaning storage volume. Ideally it would need 2 stages with pH control. Google for it
Electro-chemist, author of "Making profit from chemistry of precious metals
in the scrapyard" - 30 and more recovery procedures with full ecological solutions.
20 pages. "Gold electronic enigma, 1, 2 or 3. A look inside the electronic shell of 9 noble metals" - explaining conductivity, superconductivity, colors, formation and many more...36 pages.
Look for "Everymetalchemistry" on facebook.
http://www.facebook.com/Everymetalchemistry

Goldextraction32
Member
Posts: 7
Joined: September 16th, 2018, 12:37 pm
Country of Origin: India

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Goldextraction32 » September 17th, 2018, 6:34 am

Platinum wrote:I'm also a member over at 911 Metallurgist. Is this the same discussion from over there about the gold fingers?

No, it is not. Thanks for your concern.


User avatar
Platinum
Active Member
Posts: 57
Joined: January 3rd, 2008, 4:26 pm
Location: Earth

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Platinum » September 17th, 2018, 9:12 am

Goldextraction32 wrote:
Platinum wrote:I'm also a member over at 911 Metallurgist. Is this the same discussion from over there about the gold fingers?

No, it is not. Thanks for your concern.



Hummmmmm.........
You do not have the required permissions to view the files attached to this post.
The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C[1].M Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/lndylk
4. Chemistry Handbooks Here (FREE) >> http://tinyurl.com/n27pqu
ALL FREE-----ALL THE TIME

Goldextraction32
Member
Posts: 7
Joined: September 16th, 2018, 12:37 pm
Country of Origin: India

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Goldextraction32 » September 17th, 2018, 10:38 am

Lino1406 wrote:Hypochlorite will destroy cyanide. (Air) mixing and enough time - meaning storage volume. Ideally it would need 2 stages with pH control. Google for it

Thanks for your reply. Can you describe it in detail?

User avatar
Platinum
Active Member
Posts: 57
Joined: January 3rd, 2008, 4:26 pm
Location: Earth

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Platinum » September 17th, 2018, 3:28 pm

So your just going to ignore this situation here like you did over there aren't you?
Is that or is that not your post?
The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C[1].M Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/lndylk
4. Chemistry Handbooks Here (FREE) >> http://tinyurl.com/n27pqu
ALL FREE-----ALL THE TIME

User avatar
FrugalRefiner
Active Member
Posts: 3603
Joined: January 14th, 2012, 5:06 pm
Country of Origin: USA
Location: Ohio, USA

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby FrugalRefiner » September 17th, 2018, 7:51 pm

Goldextraction, I've read your post here and the post Platinum shared from another forum.

Your post here
The post Platinum shared

We have a gold cyanide solution of 28 liters.
We have a gold cyanide solution of 30 liters.

We removed gold from gold plated connectors.
We removed gold from gold fingers.

We used 475 grams of commercial grade sodium cyanide and 5 liters of hydrogen peroxide of 36%.
We used 500 grams of commercial grade sodium cyanide and 1.5 liters of hydrogen peroxide of 36%.

This solution contains 100 grams of gold & around 5 grams of iron.
This solution contains 100 grams of gold and around 5 grams of iron and 5 grams of solder.

Can sodium cyanide and hydrogen peroxide be destructed using copper sulfate & sodium metabisulfite ?
We want to use copper sulphate, sodium metabisulfite for cyanide and hydrogen peroxide destruction.

How to proceed about it?
How to proceed about it?

There are just too many similarities. I don't care if you posted the same question somewhere else. I do care if you deny it. Be honest, and our members will try to help you.

Dave
Printer friendly copy of C. M. Hoke's Refining Precious Metal Wastes.
Screen readable copy of C. M. Hoke's Refining Precious Metal Wastes.

User avatar
Platinum
Active Member
Posts: 57
Joined: January 3rd, 2008, 4:26 pm
Location: Earth

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Platinum » September 17th, 2018, 8:15 pm

He got answers over there, he's just price shopping for a better one to fit what he wants to hear instead of what he needs to hear. If he would do a little research the answer is here on the forum.
The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C[1].M Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/lndylk
4. Chemistry Handbooks Here (FREE) >> http://tinyurl.com/n27pqu
ALL FREE-----ALL THE TIME

User avatar
goldsilverpro
Active Member
Posts: 7938
Joined: March 30th, 2007, 4:45 pm
Country of Origin: USA
Location: Benton, Arkansas

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby goldsilverpro » September 17th, 2018, 9:19 pm

Dupont once published a cyanide destruct method using hydrogen peroxide.
"Everything should be as simple as possible, but not simpler" - Albert Einstein
"It is better to hear the rebuke of the wise, than for a man to hear the song of fools" Ecc 7:5, 1611 AV
"The refiner is always the last liar." Louis Labash, 1979

GoldSilverPro's eBook For Sale. viewtopic.php?f=84&t=22327&p=233617#p233617
GSP Consulting viewtopic.php?f=84&t=26425

Goldextraction32
Member
Posts: 7
Joined: September 16th, 2018, 12:37 pm
Country of Origin: India

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Goldextraction32 » September 18th, 2018, 6:31 am

Platinum wrote:So your just going to ignore this situation here like you did over there aren't you?
Is that or is that not your post?

In fact we were two partners in gold recovery business. That is the reason our post started with “we have……” We had some issues and separated . And that solution became my property. And I don’t understand this gold recovery line as much as my partner did. The first question was posted by my partner. And the question on Gold refining forum is posted by me. I made little bit of changes because I thought people would not be interested to answer the same question. But honestly speaking no dishonest intentions were meant. If my post disturbed anyone, I am sorry about that. I was so tensed I even forgot to start this post with I have…… this time because my gold is stuck in the solution.
So, this is the truth. Please help !
Last edited by Goldextraction32 on September 18th, 2018, 8:09 am, edited 1 time in total.

Goldextraction32
Member
Posts: 7
Joined: September 16th, 2018, 12:37 pm
Country of Origin: India

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Goldextraction32 » September 18th, 2018, 6:43 am

FrugalRefiner wrote:Goldextraction, I've read your post here and the post Platinum shared from another forum.

Your post here
The post Platinum shared

We have a gold cyanide solution of 28 liters.
We have a gold cyanide solution of 30 liters.

We removed gold from gold plated connectors.
We removed gold from gold fingers.

We used 475 grams of commercial grade sodium cyanide and 5 liters of hydrogen peroxide of 36%.
We used 500 grams of commercial grade sodium cyanide and 1.5 liters of hydrogen peroxide of 36%.

This solution contains 100 grams of gold & around 5 grams of iron.
This solution contains 100 grams of gold and around 5 grams of iron and 5 grams of solder.

Can sodium cyanide and hydrogen peroxide be destructed using copper sulfate & sodium metabisulfite ?
We want to use copper sulphate, sodium metabisulfite for cyanide and hydrogen peroxide destruction.

How to proceed about it?
How to proceed about it?

There are just too many similarities. I don't care if you posted the same question somewhere else. I do care if you deny it. Be honest, and our members will try to help you.

Dave

In fact we were two partners in gold recovery business. That is the reason our post started with “we have……” We had some issues and separated . And that solution became my property. And I don’t understand this gold recovery line as much as my partner did. The first question was posted by my partner. And the question on Gold refining forum is posted by me. I made little bit of changes because I thought people would not be interested to answer the same question. But honestly speaking no dishonest intentions were meant. If my post disturbed someone, I am sorry for that. I was so tensed I even forgot to start this post with I have…… this time because my gold is stuck in the solution.
So, this is the truth. Please help !
Last edited by Goldextraction32 on September 18th, 2018, 8:10 am, edited 1 time in total.

Lino1406
Active Member
Posts: 1249
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Lino1406 » September 18th, 2018, 7:15 am


Goldextraction32
Member
Posts: 7
Joined: September 16th, 2018, 12:37 pm
Country of Origin: India

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Goldextraction32 » September 18th, 2018, 8:08 am

Lino1406 wrote:https://www.emerson.com/documents/automation/application-data-cyanide-destruction-monitoring-ph-orp-en-68412.pdf is an example

Thanks for the link.
Can we destroy cyanide by simply adding H2O2 to the solution ? Is it safe ? What will be the reaction ? How to determine all the cyanide has been destroyed?
Thanks!

Lino1406
Active Member
Posts: 1249
Joined: November 1st, 2007, 12:56 pm
Country of Origin: Israel
Location: Israel
Contact:

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Lino1406 » September 18th, 2018, 8:39 am

H2O2 with cyanide will result in some kind of "fertilizer". Each result has its dangers. I suggest you to study the subject more seriously or get a quotation from a company and not to expect magic recipes.

User avatar
Platinum
Active Member
Posts: 57
Joined: January 3rd, 2008, 4:26 pm
Location: Earth

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Platinum » September 18th, 2018, 9:12 am

Goldextraction32 wrote:
Platinum wrote:So your just going to ignore this situation here like you did over there aren't you?
Is that or is that not your post?

In fact we were two partners in gold recovery business. That is the reason our post started with “we have……” We had some issues and separated . And that solution became my property. And I don’t understand this gold recovery line as much as my partner did. The first question was posted by my partner. And the question on Gold refining forum is posted by me. I made little bit of changes because I thought people would not be interested to answer the same question. But honestly speaking no dishonest intentions were meant. If my post disturbed anyone, I am sorry about that. I was so tensed I even forgot to start this post with I have…… this time because my gold is stuck in the solution.
So, this is the truth. Please help !


Not a problem sir. Just trying to figure things out.
The difference between stupidity and genius is that genius has its limits. Albert Einstein
1. Refining Precious Metal Wastes C[1].M Hoke http://tinyurl.com/mfnyhs
(REV) (Free Download)
2. Get the (FREE) Gold Refining Forum Handbook VOL 1 here >> http://tinyurl.com/nyutnp
3. Get the (FREE) Gold Refining Forum Handbook VOL 2 (Final) here >> http://tinyurl.com/lndylk
4. Chemistry Handbooks Here (FREE) >> http://tinyurl.com/n27pqu
ALL FREE-----ALL THE TIME

kurtak
Active Member
Posts: 1647
Joined: January 16th, 2014, 12:37 pm
Country of Origin: USA
Location: Central Wisconsin

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby kurtak » September 18th, 2018, 10:42 am

Goldextraction32 wrote:We have a gold cyanide solution of 28 liters. We removed gold from gold plated connectors. We used 475 grams of commercial grade sodium cyanide and 5 liters of hydrogen peroxide of 36%. This solution contains 100 grams of gold & around 5 grams of iron. Can sodium cyanide and hydrogen peroxide be destructed using copper sulfate & sodium metabisulfite ? Or there could be a better solution ? How much quantity of chemical/chemicals will be used to destroy sodium cyanide and hydrogen peroxide? How to proceed about it?
Please Help !



Per the underlined - is the gold still in solution ?


I ask - because you are asking how to "destroy" the cyanide --- which would be a question of what to do with the solution (cyanide) AFTER you have recovered the gold


If the gold is still in solution - then your question needs to be --- how do I "recover" the gold from my cyanide solution


copper sulfate &/or sodium metabisulfite will not recover the gold from your cyanide solution - nor will it distroy the cyanide AFTER you recover the gold

So - what do you want to do

destroy the cyanide after the gold has already been recovered - OR ------

recover the gold - the cyanide can &/or needs to be destroyed "after" the gold is recovered


WARNING - do not add acid to cyanide --- you WILL die


do NOT have your cyanide in the the same work area that have acids in the same work area - you may (very well) die


keep cyanide & acids in seperate work areas

Kurt

kurtak
Active Member
Posts: 1647
Joined: January 16th, 2014, 12:37 pm
Country of Origin: USA
Location: Central Wisconsin

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby kurtak » September 18th, 2018, 10:55 am

Added Note; - if you need to recover the gold - lets talk about that "first" --- then we can talk about destroying the cyanide

Don't do ANYTHING until you/we know exactly what you are doing &/or until you FULLY understand it

we have several members that can/will help you - but we/you "need" details

Kurt

Goldextraction32
Member
Posts: 7
Joined: September 16th, 2018, 12:37 pm
Country of Origin: India

Re: How to destroy sodium cyanide & hydrogen peroxide

Postby Goldextraction32 » September 18th, 2018, 12:26 pm

kurtak wrote:Added Note; - if you need to recover the gold - lets talk about that "first" --- then we can talk about destroying the cyanide

Don't do ANYTHING until you/we know exactly what you are doing &/or until you FULLY understand it

we have several members that can/will help you - but we/you "need" details

Kurt

Thanks for your reply.
My gold is still in the solution. I want to first recover gold and then destroy cyanide. Please advise how to proceed? Recover gold first and then destroy cyanide or destroy cyanide first and then recover gold?
Thanks!


Return to “Chemical Processes”

Who is online

Users browsing this forum: Wyndham and 0 guests