G gulammohd Member Joined Feb 20, 2022 Messages 8 Location Ahmedabad Apr 28, 2022 #1 Which precious metals are used in electronics that can be recovered
N nickvc Moderator Staff member Moderator Joined Sep 14, 2009 Messages 5,544 Location birmingham Apr 28, 2022 #2 Gold is the most likely to be encountered some silver is possible but PGMs are not common in most items available to the average refiner .
Gold is the most likely to be encountered some silver is possible but PGMs are not common in most items available to the average refiner .