pilotdan
Active member
Hi all,
I must be missing something. I am really surprised at what memory lots sell for on eBay. I sampled several lots and put the data into a spreadsheet and came up with $8.29 a pound which included shipping.
Ebay# Weight Price Shipping Total Price / LB
250224259605 5.00 $40.00 $14.12 $54.12 $10.82
170202830473 20.00 $122.50 $18.00 $140.50 $7.03
230234204330 50.00 $350.00 $34.95 $384.95 $7.70
140217262502 12.00 $75.00 $19.00 $94.00 $7.83
370031620404 22.00 $170.49 $10.00 $180.49 $8.20
110234980325 17.00 $125.00 $10.00 $135.00 $7.94
260219226810 22.00 $171.50 $26.11 $197.61 $8.98
300205230387 20.00 $150.00 $25.00 $175.00 $8.75
370029022217 21.70 $150.27 $10.00 $160.27 $7.39
$8.29 Avg / LB
The interesting thing I found was that many buyers have been buying at these high prices for a while. Do they know something I don't? One buyer I found has been buying these lots for the last 90 days. (90 days is the max amount of buying data you can view on ebay)
Thought's?
Sorry about the formatting of the data. I could not figure out how to get it to keep its formatting.
If this is not in the appropriate place, please move it.
I must be missing something. I am really surprised at what memory lots sell for on eBay. I sampled several lots and put the data into a spreadsheet and came up with $8.29 a pound which included shipping.
Ebay# Weight Price Shipping Total Price / LB
250224259605 5.00 $40.00 $14.12 $54.12 $10.82
170202830473 20.00 $122.50 $18.00 $140.50 $7.03
230234204330 50.00 $350.00 $34.95 $384.95 $7.70
140217262502 12.00 $75.00 $19.00 $94.00 $7.83
370031620404 22.00 $170.49 $10.00 $180.49 $8.20
110234980325 17.00 $125.00 $10.00 $135.00 $7.94
260219226810 22.00 $171.50 $26.11 $197.61 $8.98
300205230387 20.00 $150.00 $25.00 $175.00 $8.75
370029022217 21.70 $150.27 $10.00 $160.27 $7.39
$8.29 Avg / LB
The interesting thing I found was that many buyers have been buying at these high prices for a while. Do they know something I don't? One buyer I found has been buying these lots for the last 90 days. (90 days is the max amount of buying data you can view on ebay)
Thought's?
Sorry about the formatting of the data. I could not figure out how to get it to keep its formatting.
If this is not in the appropriate place, please move it.