Absolutsecurity Well-known member Joined Jan 4, 2008 Messages 191 Location Tehachapi, CALIFORNIA Jan 20, 2008 #1 Does anyone think an old assay crucible would hold any PM - the thing has the tell tale purple as well as some gold sparkels on it? Might be better just to keep as an antique HUH!! Glynn Attachments 98859466_tp.jpg 12.5 KB · Views: 322
Does anyone think an old assay crucible would hold any PM - the thing has the tell tale purple as well as some gold sparkels on it? Might be better just to keep as an antique HUH!! Glynn
lazersteve Well-known member Joined Feb 27, 2007 Messages 7,334 Location Florida Jan 20, 2008 #2 Glynn, Crucibles will definitely hold PMs, , both on the surface and in the structures nooks and crannys. Steve
Glynn, Crucibles will definitely hold PMs, , both on the surface and in the structures nooks and crannys. Steve
Absolutsecurity Well-known member Joined Jan 4, 2008 Messages 191 Location Tehachapi, CALIFORNIA Jan 20, 2008 #3 Might be a shame to crush one up - Its like its allready seasoned and full of really old 100 year old + ancient miners spoils! G
Might be a shame to crush one up - Its like its allready seasoned and full of really old 100 year old + ancient miners spoils! G