After two years of collecting, experimenting, and general frustration, my "First-born arrived 7/20/07. This 6.8 gram "'Lil Nugget" is the result of combining 3 pounds 7 ounces of mixed fingers and the application of AP and HCl/Clorox methods, found in this incredible forum. There is no way to express my gratitude to all of you who have helped and encouraged me through the process..Thank you all.
Mike