I guess he is doing tests to get familiar with the reactions.Imo, you just wasting the acid by neutralizing it when you can get precious nitrate if you just pour copper till you free of acid and can get nitrate.
Yup - zinc powderSo you can use Zinc and Sulfuric?
Sure. Silver Chloride in your glass jar with weak warm Sulphuric. Add a small amount of Zinc powder and stir. Use your common sense and don't over add it and convert. It's instant. Once it's all converted and hopefully with very little excess you can clean with HCl as required.Never ran across the zinc method. Any details for it.
it is enough to have a small piece of silver.I have dissolved some pure silver using nitric acid, I started of with a solution(approx 5ml) of nitric acid and distilled water with a pH of 1, after dissolving some silver approx(1.25-1.5g) with some silver still at the bottom the pH has dropped to close to 5.
I was wondering what should be the pH of the solution before I start cementing the silver using copper.