What is the highest yield you have found with fingers?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

skyline27

Well-known member
Joined
Jul 26, 2007
Messages
294
Location
Wisconsin
ViewItem&item=150209474440&ssPageName=ADME:B:WNA:US:1123

This 3 pound lot of fingers recently sold for $222 plus shipping. \
$70+ per pound!!!

I
t would need to yield about 3 grams per pound to break even. Are there fingers that have this much gold content?
 
Scrapman,

Did you weigh the gold in the photo or did you weigh the button after it was melted? There is a big difference in the weights.

If that is the final button weight what was the source material of the fingers?