I added a new video on my website today.
The video demonstrates the precipitation of 40 grams of dissolved platinum using potassium chloride.
Here's a photo of the money shot:
You can find the video on my website in the PGMs section.
GoldRecovery.US
Please post your comments here.
Steve
The video demonstrates the precipitation of 40 grams of dissolved platinum using potassium chloride.
Here's a photo of the money shot:
You can find the video on my website in the PGMs section.
GoldRecovery.US
Please post your comments here.
Steve