Hi everyone,
I'm new to gold refining and I've collected a decent amount of electronic scrap. After talking to a local supplier of scrap he gave me a solution recipe to extract the gold. The solution calls for a 70% sodium cyanide, 10% sodium hydroxide mix but I can't find a cheap supplier without buying bulk. Any info on where I could look without paying out the a$$ for regaent grade
Thanks
I'm new to gold refining and I've collected a decent amount of electronic scrap. After talking to a local supplier of scrap he gave me a solution recipe to extract the gold. The solution calls for a 70% sodium cyanide, 10% sodium hydroxide mix but I can't find a cheap supplier without buying bulk. Any info on where I could look without paying out the a$$ for regaent grade