so the Forum books indicates that it's best to dissolve the base Metals first before dissolving the gold and you can do that with acid peroxide. So my question is:
- if I had already made the mistake and recovered the gold along with other base metals in powder form can anyone confirm if I am right in assuming that if I add acid peroxide to the powder I should be able to dissolve only the base Metals & the powder left undissolved should be the gold is that correct?
- if I had already made the mistake and recovered the gold along with other base metals in powder form can anyone confirm if I am right in assuming that if I add acid peroxide to the powder I should be able to dissolve only the base Metals & the powder left undissolved should be the gold is that correct?