  1. B

    Separating Pd and Ag from Tungsten filaments

    We have about 80+ lbs. of pure Tungsten filaments used to evaporate an 80( Ag )/20( Pd ) alloy. The residue of Pd/Ag is about 3-4% by weight. What is the best method to strip the Pd & Ag and preserving the Tungsten metal for separate recycling ? Then , how best to separate the Pd and Ag into...
  2. D

    Rh and Pd extraction and separation

    Hi dear, I read some of your topics on the forum about handling rhodium and palladium and respectfully I would like to know if you could instruct me. I have approximately 20 kg of scrap from galvanic processes plated with Rh and Pd in the final layer, and the lower ones are copper and tin and...
  3. chris1977impala1

    (Help!!!) (Platinum?) (Palladium)? (Copper?) (Rodium?) Stanous Chloride Test? Catalytic converter chlorine leach solution?

    can somebody please tell me what I have in solution? This is a status chloride test That I used on a catalytic converter. Substrate chlorine leach solution!
  4. D

    Separation of PGM's by Photocatalysis in Anatase Titanium Dioxide

    Hello my friends, I was looking for files about pgm's and I came across this document, I hope to contribute positively to the forum, I await your opinion
  5. 100tific

    Chemical Recovering Palladium

    hi guys, i was profilling the recovering palladium method and i found some problems. I have an alloy wich has gold, silver and palladium. i inquarted with copper to low the silver concentration down to 8% and laminate de ingot. Then i dissolved the alloy in AR and i filtered to separate the...