  1. U

    Gold precipitating agents/methods

    Anybody with experience or thorough testing of various precipitating agents that could help me determine best gold precipitation methods or agents? I have heard SMB is very good, but I've also heard about various other such as FeSO4, Na2S, Ascorbic acid, Zinc, SO2 gas, Activated Carbon. These...
  2. 100tific

    Recovering Palladium

    hi guys, i was profilling the recovering palladium method and i found some problems. I have an alloy wich has gold, silver and palladium. i inquarted with copper to low the silver concentration down to 8% and laminate de ingot. Then i dissolved the alloy in AR and i filtered to separate the...