  1. Will

    Help with refining 10k to 24k gold

    I am a new member. I am trying to refine 84g of 10k gold. I melted the gold and poured it into water to get it into smaller pieces. I the put the gold in 3oz of nitric, left it for a couple hours and then added the nitric acid to 9oz of hydrochloric acid. We then let it sit for 40 hours. It...